Carbon Black ASTM D1603
Carbon black content test device is designed and produced in line with GB/T2951.41 - 2008 <Common test methods for insulating and sheathing materials of electric and optical cables--Part 41: Methods specific to polyethylene and polypropylene compounds - Carbon black and/or mineral filler content measurement in polyethylene by direct combustion>, used for determination of carbon black content in polyethylene, polypropylene, polybutene plastics.
Test Procedure:
A sample of known weight is placed into a weighed combustion boat. The sample is then placed into a 600°C tube furnace under a dry oxygen free Nitrogen purge. After a set time the combustion boat with the burn residue is cooled under the nitrogen purge and weighed. The combustion boat is then placed into a 600°C muffle furnace to oxidize the carbon residue. When the carbon is completely oxidized the combustion boat is cooled and weighed.
Data:
Carbon black content = (B-C)/A*100%;
Mineral filler content = C/A*100%;
The content of the filler = B/A*100%.
B = the mass of the residue from the tube furnace
C= the mass of the residue from the muffle furnace
A= the original mass of the sample
Technical Parameter:
Tubular Electric Furnace: RT ~ 800 ℃, Length 400mm
Quartz Tube: Inner diameter 30mm, overall length 600mm
Temperature Sensor: K-type, RT~ 1300 ℃
Washing Bottle: 500ml, 2 pcs / unit
Combustion Boat: 77 type, 100 pcs / unit
Flowmeter: 0.3 ~ 3L / min
Specification:
Overall Dimensions: 600mm (W) * 450mm (D) * 770mm(H)
Power Supply: AC220V 50 / 60Hz
Gas Source: nitrogen (oxygen content <0.5%), oxygen (provided by customers)
Carbon Black Content Test Device
Carbon Black ASTM D1603
Carbon black content test device is designed and produced in line with GB/T2951.41 - 2008 <Common test methods for insulating and sheathing materials of electric and optical cables--Part 41: Methods specific to polyethylene and polypropylene compounds - Carbon black and/or mineral filler content measurement in polyethylene by direct combustion>, used for determination of carbon black content in polyethylene, polypropylene, polybutene plastics.
Test Procedure:
A sample of known weight is placed into a weighed combustion boat. The sample is then placed into a 600°C tube furnace under a dry oxygen free Nitrogen purge. After a set time the combustion boat with the burn residue is cooled under the nitrogen purge and weighed. The combustion boat is then placed into a 600°C muffle furnace to oxidize the carbon residue. When the carbon is completely oxidized the combustion boat is cooled and weighed.
Data:
Carbon black content = (B-C)/A*100%;
Mineral filler content = C/A*100%;
The content of the filler = B/A*100%.
B = the mass of the residue from the tube furnace
C= the mass of the residue from the muffle furnace
A= the original mass of the sample
Technical Parameter:
Tubular Electric Furnace: RT ~ 800 ℃, Length 400mm
Quartz Tube: Inner diameter 30mm, overall length 600mm
Temperature Sensor: K-type, RT~ 1300 ℃
Washing Bottle: 500ml, 2 pcs / unit
Combustion Boat: 77 type, 100 pcs / unit
Flowmeter: 0.3 ~ 3L / min
Specification:
Overall Dimensions: 600mm (W) * 450mm (D) * 770mm(H)
Power Supply: AC220V 50 / 60Hz
Gas Source: nitrogen (oxygen content <0.5%), oxygen (provided by customers)
Site Map
Copyright © 2018 Chongqing Gold Mechanical & Electrical Equipment Co.,Ltd. All Rights Reserved.